General
Dimension
Property | Value |
---|---|
Width | 1500 mm Show Supplier Material materials with Width of 1500 mm |
Dimensions | Standard stock sizes: 1540mm x 3048mm and 10-50mm in thickness |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 70 GPa Show Supplier Material materials with Elastic modulus of 70 GPa | |
Elongation A5 | 23.0 °C | 2.5 - 4.5 % Show Supplier Material materials with Elongation A5 of 2.5 - 4.5 % | |
Hardness, HBW | 23.0 °C | 110 - 120 [-] Show Supplier Material materials with Hardness, HBW of 110 - 120 [-] | Test method: 2.5/62.5 |
Tensile strength | 23.0 °C | 320 - 380 MPa Show Supplier Material materials with Tensile strength of 320 - 380 MPa | |
Yield strength Rp0.2 | 23.0 °C | 290 - 340 MPa Show Supplier Material materials with Yield strength Rp0.2 of 290 - 340 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.3E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.3E-5 1/K |
Specific heat capacity | 23.0 °C | 875 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 875 J/(kg·K) |
Thermal conductivity | 23.0 °C | 125 - 155 W/(m·K) Show Supplier Material materials with Thermal conductivity of 125 - 155 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 2.10E+7 - 2.40E+7 S/m Show Supplier Material materials with Electrical conductivity of 2.10E+7 - 2.40E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Heat treatable alloy | |
Processing history | Temper: T79, solution heat treated, quenched, artificially aged |