Ceramic Carbon Composite CARBOPRINT® Si1

Ceramic Carbon Composite CARBOPRINT® Si2

Ceramic Carbon Composite CARBOPRINT® Si3

Search results

Materials

Available properties

General

Porosity (%)
Density (g/cm³)

Mechanical

Elastic modulus (GPa)
Flexural strength (MPa)

Thermal

Coefficient of thermal expansion (1/K)
Thermal conductivity (W/(m·K))

Electrical

Electrical resistivity (Ω·m)

You should select at least 1 property to see the chart!

Ceramic Carbon Composite CARBOPRINT® Si1

Ceramic Carbon Composite CARBOPRINT® Si2

Ceramic Carbon Composite CARBOPRINT® Si3

Primary standard name

Equivalent standard names

Related standards

Chemical composition

Element

Weight %

Comment

Element

Weight %

Comment

Element

Weight %

Comment

Material Information

Processing methods

The CARBOPRINT family combines our comprehensive carbon material know-how with additive manufacturin

More

The CARBOPRINT family combines our comprehensive carbon material know-how with additive manufacturin

More

The CARBOPRINT family combines our comprehensive carbon material know-how with additive manufacturin

More

Secondary Phase

Mechanical

Elastic modulus, E

70 GPa at 23 °C

95 GPa at 23 °C

100 GPa at 23 °C

Flexural strength, σbend

65 MPa at 23 °C

75 MPa at 23 °C

110 MPa at 23 °C

General

Porosity, Vvoid

0.1 %

0.1 %

0.1 %

Density, ρ

2.2 g/cm³ at 23 °C

2.4 g/cm³ at 23 °C

2.3 g/cm³ at 23 °C

Electrical

Electrical resistivity, ρel

3E-5 Ω·m at 23 °C

1E-4 Ω·m at 23 °C

4E-5 Ω·m at 23 °C

Thermal

Coefficient of thermal expansion, α

3E-6 1/K at 200 °C

3E-6 1/K at 200 °C

3E-6 1/K at 200 °C

Thermal conductivity, λ

40 W/(m·K) at 23 °C

60 W/(m·K) at 23 °C

80 W/(m·K) at 23 °C