Unclassified Low Alloy Steel
EN 10225 Grade S420G1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10225 Grade S355G7 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10225 Grade S420G1 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10225 Grade S460G1 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10225 Grade S355G13 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10225 Grade S355G13 quenched and tempered (+QT)Medium Carbon Steel
EN 10225 Grade S355G14 normalized or normalized formed (+N)Medium Carbon Steel
EN 10225 Grade S355G15 normalized or normalized formed (+N)Medium Carbon Steel
EN 10225 Grade S355G14 quenched and tempered (+QT)Medium Carbon Steel
EN 10225 Grade S355G15 quenched and tempered (+QT)Wrought Copper Pure / Low Alloyed Copper
BS 2875 Grade C 105Wrought Copper Pure / Low Alloyed Copper
BS 2871-2 Grade C 107Cast Copper Brass Yellow Brass
PN/H 87026 Grade CC762SCast Copper Brass Yellow Brass
PN/H 87026 Grade CB762SUnclassified Low Alloy Steel
EN 10225 Grade S355G10 normalized or normalized formed (+N)Unclassified Low Alloy Steel
EN 10225 Grade S355G10 thermomechanically rolledUnclassified Low Alloy Steel
EN 10225 Grade S355G11 as-rolled condition (+AR)Unclassified Low Alloy Steel
EN 10225 Grade S355G11 normalized or normalized formed (+N)Unclassified Low Alloy Steel
EN 10225 Grade S355G11 thermomechanically rolledUnclassified Low Alloy Steel
EN 10225 Grade S355G12 as-rolled condition (+AR)