Antimon: 0.7 - 0.8 %

Quick Comparison

Pure/Low Alloyed Lead

DIN 17640-2 Grade 081K

Leaded Tin Bronze

ASTM B505 Grade C93800

Leaded Tin Bronze

ASTM B505 Grade C94100

Leaded Tin Bronze

ASTM B505 Grade C94300

Leaded Tin Bronze

ASTM B505 Grade C93800

Leaded Tin Bronze

ASTM B505 Grade C94100

Leaded Tin Bronze

ASTM B505 Grade C94300

Leaded Tin Bronze

ASTM B584 Grade C93800

Leaded Tin Bronze

ASTM B584 Grade C94300

Pure/Low Alloyed Lead

EN 12548 Grade PB081K

Wrought Copper Bronze Aluminium Bronze

ISO 1338 Grade CuAl10Fe5Ni5

Leaded Tin Bronze

ASTM B30 Grade C94500

Leaded Tin Bronze

AS/NZS 1565 Grade C94100

Leaded Tin Bronze

ASTM B30 Grade C94400

Leaded Tin Bronze

NS 16544 Grade CC497K
Seite 1 von 2