Coefficient of friction, static: 0.38 [-]

Quick Comparison

Polyamide 610 (PA610)

LNP™ LUBRICOMP™ Compound QFL32

Geliefert von:

Sabic

Polyphthalamid (PPA)

LNP™ LUBRICOMP™ Compound UFL269SA

Geliefert von: