Coefficient of friction, static: 0.55 [-]

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2750-01

Geliefert von:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2950-05

Geliefert von:

Arkema: High Performance Polymers

High Impact Polystyrene (HIPS)

LNP™ LUBRICOMP™ Compound CG006

Geliefert von:

Sabic