Creep strength 10^4 cycles: 226 MPa

Quick Comparison

Unclassified Low Alloy Steel

EN 10028-5 Grade P420MHTL2

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10028-5 Grade P420K4

Geliefert von: