Hardness, Rockwell F: 92 [-]

Quick Comparison

Wrought Copper Nickel Silver Grade

ASTM B122 Grade C77000 OS015

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C10100 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C10100 H06

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C10100 H10

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C10800 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C10800 H08

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C11000 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C11000 H08

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C11300 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C11300 H08

Wrought Copper Nickel Silver Grade

ASTM B122 Grade C75200 OS015

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C10300 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C10300 H10

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C12000 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C12000 H06

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C12000 H08

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C12000 H10

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C12300 H06

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C12300 H08

Wrought Copper Pure / Low Alloyed Copper

ASTM B152 Grade C12300 H10