Hardness, Rockwell Superficial 15-N: 77 [-]

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B194 Grade C17000 TH01

Wrought Copper High Copper Alloy

ASTM B194 Grade C17000 TF00