Heat deflection temperature, 0.45 MPa: 198 °C

Quick Comparison

Polyetherimid (PEI)

ULTEM™ Resin 1000E - Europe

Geliefert von:

Sabic

Polyetherimid (PEI)

ULTEM™ Resin 1000EF - Europe

Geliefert von:

Sabic

Polyetherimid (PEI)

ULTEM™ Resin 1000EF - Asia

Geliefert von:

Sabic

Polyetherimid (PEI)

ULTEM™ Resin 1000EF - Americas

Geliefert von:

Sabic

Polybutylenterephthalat (PBT)

VALOX™ Resin 732E