Heat deflection temperature, 1.80 MPa: 179 °C

Quick Comparison

Polysulfon (PSU)

LNP™ THERMOCOMP™ Compound GF003

Geliefert von:

Sabic

Polymermischung (Blend)

LNP™ STAT-LOY™ Compound 9X03508

Geliefert von:

Sabic

Polyetheretherketon (PEEK)

LNP™ THERMOCOMP™ Compound LF002XXP-WT02005

Geliefert von:

Sabic