Heat deflection temperature, 1.80 MPa: 291 °C

Quick Comparison

Polyetheretherketon (PEEK)

LNP™ STAT-KON™ Compound LX00797C

Geliefert von:

Sabic

Polyetheretherketon (PEEK)

LNP™ STAT-KON™ Compound LX00486C

Geliefert von:

Sabic