High Amp Arc Ignition: 2.3 mm

Quick Comparison

Polycarbonat (PC)

LEXAN™ Copolymer EXL9330 - Europe

Geliefert von:

Sabic

Polycarbonat (PC)

LEXAN™ Copolymer EXL9330 - Asia

Geliefert von:

Sabic

Polycarbonat (PC)

LEXAN™ Copolymer EXL9330 - Americas

Geliefert von:

Sabic