Impact strength, Izod unnotched, ASTM: 453 J/m

Quick Comparison

Polycarbonat (PC)

LNP™ STAT-KON™ Compound DE0029E

Geliefert von:

Sabic

Polyamide 11 (PA11)

LNP™ LUBRICOMP™ Compound HFG25Z

Geliefert von:

Sabic

Polyphthalamid (PPA)

LNP™ LUBRICOMP™ Compound UL002S

Geliefert von:

Sabic