Impact strength, Izod unnotched, ASTM: 704 J/m

Quick Comparison

Polyamide 66 (PA66)

LNP™ STAT-KON™ Compound RE0039

Geliefert von:

Sabic

Polyetheretherketon (PEEK)

LNP™ THERMOCOMP™ Compound LC008E - Asia

Geliefert von:

Sabic

Polyetheretherketon (PEEK)

LNP™ THERMOCOMP™ Compound LC008E - Americas

Geliefert von:

Sabic