Impact strength, Izod unnotched, ASTM: 880 J/m

Quick Comparison

Polybutylenterephthalat (PBT)

VALOX™ Resin 4031

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFL36U

Geliefert von:

Sabic

Polybutylenterephthalat (PBT)

LNP™ LUBRICOMP™ Compound WL002

Geliefert von: