Plane-Strain Fracture Toughnes: 10.4 MPa·√m

Quick Comparison

Cobalt Matrix Composite

CTS20D

Geliefert von:

CERATIZIT

Cobalt Matrix Composite

CTM14E (cemented carbide)

Geliefert von: