Plane-Strain Fracture Toughnes: 8.7 MPa·√m

Quick Comparison

Cobalt Matrix Composite

CTS17R (cemented carbide)

Geliefert von:

CERATIZIT

Cobalt Matrix Composite

CTS08M (cemented carbide)

Geliefert von: