Alphalegierung
UNS R56320Alphalegierung
UNS R56320Alphalegierung
UNS R56320Alphalegierung
UNS R56320Wrought Copper Brass Yellow Brass
EN 12163 Grade CuZn20 R360Wrought Copper Brass Yellow Brass
EN 12166 Grade CuZn20 R260Wrought Copper Brass Yellow Brass
EN 12163 Grade CuZn20 R450Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn20 G010Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn20 G020Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn20 G035Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn20 R270Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn20 R320Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn20 R400Wrought Copper Brass Yellow Brass
EN 12166 Grade CuZn20 R540Wrought Copper Brass Yellow Brass
EN 12166 Grade CuZn20 H065Wrought Copper Brass Yellow Brass
EN 12163 Grade CuZn20 H140Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn20 H085Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn20 R480Wrought Copper Brass Yellow Brass
EN 12166 Grade CuZn20 H58Wrought Copper Brass Yellow Brass
EN 12166 Grade CuZn20 H165