Streckgrenze Rp0,5: 83 - 103 MPa

Quick Comparison

Cast Copper Brass Yellow Brass

ASTM B505 Grade C85700

Copper Bismuth Alloy

ASTM B584 Grade C89844

Cast Copper Brass Yellow Brass

ASTM B584 Grade C85200

Cast Copper Nickel Silver Grade

ASTM B505 Grade C97300

Cast Copper Brass Yellow Brass

ASTM B271 Grade C85200 As-Cast

Cast Copper Brass Yellow Brass

ASTM B271 Grade C85700 As-Cast

Cast Copper Nickel Silver Grade

ASTM B271 Grade C97300 As-Cast

Cast Copper Brass Yellow Brass

ASTM B505 Grade C85700