DIN 2.0550

Quick Comparison

Other Copper Zinc Alloy

EN 12164 Grade CuZn37Mn3Al2PbSi M

Wrought Copper Brass

CuZn40Al2 Hard

Geliefert von:

Salomon's Metalen

Wrought Copper Brass

CuZn40Al2 Soft

Geliefert von: