Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R590Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R540Other Copper Zinc Alloy
EN 12163 Grade CuZn40Mn2Fe1 R460Other Copper Zinc Alloy
EN 12163 Grade CuZn40Mn2Fe1 R540Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R640Other Copper Zinc Alloy
EN 12168 Grade CuZn37Mn3Al2PbSi H130Other Copper Zinc Alloy
EN 12168 Grade CuZn37Mn3Al2PbSi H150Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi H170Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R570Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R620Other Copper Zinc Alloy
EN 12163 Grade CuZn40Mn2Fe1 H110Other Copper Zinc Alloy
EN 12163 Grade CuZn40Mn2Fe1 H150Other Copper Zinc Alloy
EN 12167 Grade CuZn37Mn3Al2PbSi H160Other Copper Zinc Alloy
EN 12167 Grade CuZn40Mn2Fe1 H105Other Copper Zinc Alloy
EN 12167 Grade CuZn40Mn2Fe1 H125Other Copper Zinc Alloy
EN 12167 Grade CuZn40Mn2Fe1 R420Other Copper Zinc Alloy
EN 12167 Grade CuZn40Mn2Fe1 R470Other Copper Zinc Alloy
EN 12163 Grade CuZn40Mn2Fe1 MOther Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi MOther Copper Zinc Alloy
EN 12165 Grade CuZn40Mn2Fe1 H080