DIN 2.1090

Quick Comparison

Leaded Tin Bronze

AS/NZS 1565 Grade C92410A

Leaded Tin Bronze

AS/NZS 2738 Grade C92410

Leaded Tin Bronze

DIN 1705 Grade CC493K

Leaded Tin Bronze

DS 3001 Grade CC493K

Leaded Tin Bronze

NS 16525 Grade CC493K

Leaded Tin Bronze

SFS 2207 Grade CC493K

Leaded Tin Bronze

EN 1982 Grade CC493K

Leaded Tin Bronze

BS 1400 Grade LG4