Cast Copper Brass Yellow Brass
ASTM B22 Grade C86300 As Sand CastCast Copper Brass Yellow Brass
ASTM B505 Grade C86300Cast Copper Brass Yellow Brass
ASTM B271 Grade C86300 As-CastCast Copper Brass Yellow Brass
ASTM B505 Grade C86300Cast Copper Brass Yellow Brass
ASTM B584 Grade C86300Cast Copper Brass Yellow Brass
ASTM B763 Grade C86300 Separately Cast Test BarsCast Copper Brass Yellow Brass
JIS H5102 Grade HBSC4 MCast Copper Brass Yellow Brass
AS/NZS 1565 Grade C86300Cast Copper Brass Yellow Brass
MSZ 2675 Grade CB762SCast Copper Brass Yellow Brass
DIN 1709 Grade CC762SCast Copper Brass Yellow Brass
PN/H 87026 Grade CC762SCast Copper Brass Yellow Brass
DIN 17656 Grade CB762SCast Copper Brass Yellow Brass
PN/H 87026 Grade CB762SCast Copper Brass Yellow Brass
ISO 1338 Grade CuZn25Al6Fe3Mn3Cast Copper Brass Yellow Brass
CEN/TS 13388 Grade CC762SCast Copper Brass Yellow Brass
GOST 17711 Grade LC23A6Z3Mc2Cast Copper Brass Yellow Brass
JIS H2205 Grade HBsC In 4