Tin Brass
EN 12168 Grade CuZn37Pb1Sn1 H110Tin Brass
EN 12168 Grade CuZn37Pb1Sn1 H125Tin Brass
CEN/TS 13388 Grade CW714R R390Tin Brass
EN 12164 Grade CuZn37Pb1Sn1 R410Tin Brass
EN 12164 Grade CuZn37Pb1Sn1 R460Tin Brass
EN 12164 Grade CuZn37Pb1Sn1 R500Tin Brass
EN 12165 Grade CuZn37Pb1Sn1 H080Tin Brass
EN 12166 Grade CuZn37Pb1Sn1 R350Tin Brass
EN 12166 Grade CuZn37Pb1Sn1 R400Tin Brass
EN 12164 Grade CuZn37Pb1Sn1 R360Tin Brass
EN 12164 Grade CuZn37Pb1Sn1 R370Tin Brass
EN 12164 Grade CuZn37Pb1Sn1 R390Tin Brass
EN 12167 Grade CuZn37Pb1Sn1 H100Tin Brass
EN 12167 Grade CuZn37Pb1Sn1 H120Tin Brass
ASTM B21 Grade C48200 H04Tin Brass
ASTM B21 Grade C48200 H02Tin Brass
EN 12164 Grade CuZn37Pb1Sn1 MTin Brass
ASTM B21 Grade C48200 M30Tin Brass
ASTM B21 Grade C48200 O50Tin Brass
ASTM B21 Grade C48200 O60