Kohlenstoffarmer Stahl
ASTM A148 Grade 725-585 Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A148 Grade 795-655 Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A148 Grade 895-795 Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A148 Grade 930-860 Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A148 Grade 1035-930 Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A148 Grade 1105-1000 Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A148 Grade 1140-1035 Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A148 Grade 1140-1035L Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A148 Grade 1450-1240 Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A148 Grade 1450-1240L Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A148 Grade 1795-1450 Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A148 Grade 1795-1450L Annealed, Normalized, Normalized and Tempered, or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A148 Grade 550-275 Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered