Leaded Brass
ISO 426-2 Grade CuZn38Pb4Leaded Brass
ISO 426-2 Grade CuZn39Pb1Leaded Brass
ISO 426-2 Grade CuZn39Pb3Leaded Brass
ISO 426-2 Grade CuZn36Pb3Leaded Brass
ISO 426-2 Grade CuZn38Pb2Leaded Brass
ISO 426-2 Grade CuZn36PbLeaded Brass
ISO 426-2 Grade CuZn37Pb2Leaded Brass
ISO 426-2 Grade CuZn40Pb2Leaded Brass
ISO 426-2 Grade CuZn43Pb2Leaded Brass
ISO 426-2 Grade CuZn40Pb