Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 1.73 g/cm³ Show Supplier Material materials with Dichte of 1.73 g/cm³ | |
Partikelgrößenbereich | 0.76 µm Show Supplier Material materials with Partikelgrößenbereich of 0.76 µm | ||
Partikelgröße | max. |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 11 MPa Show Supplier Material materials with Biegefestigkeit of 11 MPa |
Biegefestigkeit, transversal | 23.0 °C | 9 MPa Show Supplier Material materials with Biegefestigkeit, transversal of 9 MPa |
Druckfestigkeit | 23.0 °C | 28 MPa Show Supplier Material materials with Druckfestigkeit of 28 MPa |
Druckfestigkeit, transversal | 23.0 °C | 28 MPa Show Supplier Material materials with Druckfestigkeit, transversal of 28 MPa |
Elastizitätsmodul | 23.0 °C | 6.87 GPa Show Supplier Material materials with Elastizitätsmodul of 6.87 GPa |
Elastizitätsmodul, transversal | 23.0 °C | 4.82 GPa Show Supplier Material materials with Elastizitätsmodul, transversal of 4.82 GPa |
Zugfestigkeit | 23.0 °C | 8 MPa Show Supplier Material materials with Zugfestigkeit of 8 MPa |
Zugfestigkeit, transversal | 23.0 °C | 7 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 7 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Aschegehalt | 23.0 °C | 7E-6 % Show Supplier Material materials with Aschegehalt of 7E-6 % | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.2E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.2E-6 1/K | average for 20-100°C |
Thermal conductivity, in-plane | 23.0 °C | 125 W/(m·K) Show Supplier Material materials with Thermal conductivity, in-plane of 125 W/(m·K) | |
Thermal conductivity, through-plane | 23.0 °C | 104 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 104 W/(m·K) | |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 2.5E-6 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 2.5E-6 1/K | average for 20-100°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 1.02E-5 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.02E-5 Ω·m |
spezifischer Widerstand, transversal | 23.0 °C | 1.37E-5 Ω·m Show Supplier Material materials with spezifischer Widerstand, transversal of 1.37E-5 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Fluidized bed reactors, Centrifugal casting molds, Large diameter molds and crucibles, Monolithic composite tooling parts, Induction and vacuum furnace parts, Heat exchangers chemical process equipment | |
Processing history | Pressure molded |