Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 1.63 g/cm³ Show Supplier Material materials with Dichte of 1.63 g/cm³ | |
Partikelgrößenbereich | 0.76 µm Show Supplier Material materials with Partikelgrößenbereich of 0.76 µm | ||
Partikelgröße | max. |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit, transversal | 23.0 °C | 13.44 MPa Show Supplier Material materials with Biegefestigkeit, transversal of 13.44 MPa |
Druckfestigkeit, transversal | 23.0 °C | 34 MPa Show Supplier Material materials with Druckfestigkeit, transversal of 34 MPa |
Elastizitätsmodul, transversal | 23.0 °C | 6.9 GPa Show Supplier Material materials with Elastizitätsmodul, transversal of 6.9 GPa |
Hardness, Rockwell R | 23.0 °C | 32 [-] Show Supplier Material materials with Hardness, Rockwell R of 32 [-] |
Zugfestigkeit, transversal | 23.0 °C | 9 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 9 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Aschegehalt | 23.0 °C | 0.12 % Show Supplier Material materials with Aschegehalt of 0.12 % | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.6E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.6E-6 1/K | average for 20-100°C |
Thermal conductivity, through-plane | 23.0 °C | 130 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 130 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand, transversal | 23.0 °C | 9.3E-6 Ω·m Show Supplier Material materials with spezifischer Widerstand, transversal of 9.3E-6 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Pressure casting molds, Centrifugal casting molds, Large diameter susceptors | |
Processing history | Pressure molded |