Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 1.83 g/cm³ Show Supplier Material materials with Dichte of 1.83 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 60 MPa Show Supplier Material materials with Biegefestigkeit of 60 MPa |
Druckfestigkeit | 23.0 °C | 100 MPa Show Supplier Material materials with Druckfestigkeit of 100 MPa |
Elastizitätsmodul | 23.0 °C | 11.5 GPa Show Supplier Material materials with Elastizitätsmodul of 11.5 GPa |
Hardness, Rockwell L | 23.0 °C | 100 [-] Show Supplier Material materials with Hardness, Rockwell L of 100 [-] |
Härte, Rockwell H | 23.0 °C | 70 [-] Show Supplier Material materials with Härte, Rockwell H of 70 [-] |
Zugfestigkeit | 23.0 °C | 40 MPa Show Supplier Material materials with Zugfestigkeit of 40 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Aschegehalt | 23.0 °C | 0.02 % Show Supplier Material materials with Aschegehalt of 0.02 % | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.2E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.2E-6 1/K | average for 20-100°C |
Thermal conductivity, in-plane | 23.0 °C | 95 W/(m·K) Show Supplier Material materials with Thermal conductivity, in-plane of 95 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 1.3E-5 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.3E-5 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Continuous casting dies, Hot pressing dies and molds | |
Processing history | Isomolded |