Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 1.82 g/cm³ Show Supplier Material materials with Dichte of 1.82 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 50 MPa Show Supplier Material materials with Biegefestigkeit of 50 MPa |
Druckfestigkeit | 23.0 °C | 85 MPa Show Supplier Material materials with Druckfestigkeit of 85 MPa |
Elastizitätsmodul | 23.0 °C | 12 GPa Show Supplier Material materials with Elastizitätsmodul of 12 GPa |
Hardness, Rockwell L | 23.0 °C | 90 [-] Show Supplier Material materials with Hardness, Rockwell L of 90 [-] |
Zugfestigkeit | 23.0 °C | 32 MPa Show Supplier Material materials with Zugfestigkeit of 32 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Aschegehalt | 23.0 °C | 0.08 % Show Supplier Material materials with Aschegehalt of 0.08 % | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.2E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.2E-6 1/K | average for 20-100°C |
Thermal conductivity, in-plane | 23.0 °C | 120 W/(m·K) Show Supplier Material materials with Thermal conductivity, in-plane of 120 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 1.05E-5 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.05E-5 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Continuous casting dies, Hot pressing dies and molds | |
Processing history | Isomolded |