Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 0.18 g/cm³ Show Supplier Material materials with Dichte of 0.18 g/cm³ |
Porosität | 90 % Show Supplier Material materials with Porosität of 90 % |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 1.1 MPa Show Supplier Material materials with Biegefestigkeit of 1.1 MPa |
Biegefestigkeit, transversal | 23.0 °C | 0.2 MPa Show Supplier Material materials with Biegefestigkeit, transversal of 0.2 MPa |
Druckfestigkeit | 23.0 °C | 0.3 MPa Show Supplier Material materials with Druckfestigkeit of 0.3 MPa |
Druckfestigkeit, transversal | 23.0 °C | 1 MPa Show Supplier Material materials with Druckfestigkeit, transversal of 1 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Aschegehalt | 23.0 °C | 0.15 % Show Supplier Material materials with Aschegehalt of 0.15 % | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.3E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.3E-6 1/K | average for 20-100°C |
Thermal conductivity, in-plane | 20.0 °C | 0.39 W/(m·K) Show Supplier Material materials with Thermal conductivity, in-plane of 0.39 W/(m·K) | |
1500.0 °C | 1.5 W/(m·K) Show Supplier Material materials with Thermal conductivity, in-plane of 1.5 W/(m·K) | ||
Thermal conductivity, through-plane | 20.0 °C | 0.18 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 0.18 W/(m·K) | |
1500.0 °C | 0.45 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 0.45 W/(m·K) | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 3E-6 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 3E-6 1/K | average for 20-100°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 6.7E-4 Ω·m Show Supplier Material materials with spezifischer Widerstand of 6.7E-4 Ω·m |
spezifischer Widerstand, transversal | 23.0 °C | 4.7E-3 Ω·m Show Supplier Material materials with spezifischer Widerstand, transversal of 4.7E-3 Ω·m |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 99.9 % Show Supplier Material materials with Kohlenstoff of 99.9 % |
Technological properties
Property | ||
---|---|---|
Application areas | Vacuum furnace insulation, Inert atmosphere furnace insulation, Inert atmosphere process equipment insulation, Semiconductor crystal growing furnace insulation | |
Processing history | Hard felt |