Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 1.62 g/cm³ Show Supplier Material materials with Dichte of 1.62 g/cm³ | |
Partikelgrößenbereich | 0.76 µm Show Supplier Material materials with Partikelgrößenbereich of 0.76 µm | ||
Partikelgröße | max. |
Mechanisch
Thermisch
Property | Temperature | Value |
---|---|---|
Aschegehalt | 23.0 °C | 0.2 % Show Supplier Material materials with Aschegehalt of 0.2 % |
Thermal conductivity, in-plane | 23.0 °C | 10 W/(m·K) Show Supplier Material materials with Thermal conductivity, in-plane of 10 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 4.19E-5 Ω·m Show Supplier Material materials with spezifischer Widerstand of 4.19E-5 Ω·m |
spezifischer Widerstand, transversal | 23.0 °C | 5E-5 Ω·m Show Supplier Material materials with spezifischer Widerstand, transversal of 5E-5 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Anodes for electrolytic processes, Applications that require low thermal conductivity material |