Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 1.74 g/cm³ Show Supplier Material materials with Dichte of 1.74 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 40 MPa Show Supplier Material materials with Biegefestigkeit of 40 MPa |
Druckfestigkeit | 23.0 °C | 65 MPa Show Supplier Material materials with Druckfestigkeit of 65 MPa |
Elastizitätsmodul | 23.0 °C | 9.5 GPa Show Supplier Material materials with Elastizitätsmodul of 9.5 GPa |
Hardness, Rockwell L | 23.0 °C | 68 [-] Show Supplier Material materials with Hardness, Rockwell L of 68 [-] |
Zugfestigkeit | 23.0 °C | 24 MPa Show Supplier Material materials with Zugfestigkeit of 24 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Aschegehalt | 23.0 °C | 0.5 % Show Supplier Material materials with Aschegehalt of 0.5 % | For applications requiring low ash, a purified version of this grade is available |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.8E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.8E-6 1/K | average for 20-100°C |
Thermal conductivity, in-plane | 23.0 °C | 120 W/(m·K) Show Supplier Material materials with Thermal conductivity, in-plane of 120 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 1.15E-5 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.15E-5 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Permanent molds, Composite tooling, Continuous casting dies, Hot pressing molds and punches, Rocket motor nozzles, Plunger and rams |