Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Partikelgröße | 30 - 100 nm Show Supplier Material materials with Partikelgröße of 30 - 100 nm | BET | |
Schüttdichte | 23.0 °C | 6.11 g/cm³ Show Supplier Material materials with Schüttdichte of 6.11 g/cm³ | |
Spezifische Oberfläche | 15 - 30 m²/g Show Supplier Material materials with Spezifische Oberfläche of 15 - 30 m²/g | BET |
Technological properties
Property | ||
---|---|---|
Application areas | proton conductor, solid oxide fuel cell, SOFC, solid electrolyte, ceramic membranes, protonic ceramic oxide fuel cell, oxide ion conductor, conductive solid electrolyte, proton ceramic electrolyzer cell, protonic ceramic membrane, proton conducting perovskite oxide, catalyst support | |
Chemical composition | BaZr0.85Y0.15O3-δ | |
Color | Fine, white powder | |
Crystal structure | Crystal structure at 25°C: Cubic perovskite, Pm-3m | |
Processing history | Cerpotech applies spray pyrolysis, a soft chemistry technique with a great potential, to produce high quality, multi-component ceramic oxide powders. With this aqueous-based environmentally friendly technology, Cerpotech is able to offer fine complex ceramic oxide powders of tailored compositions with high phase purity, high chemical purity, very high homogeneity, narrow particle distribution, offering excellent properties for further processing at competetive prices. |