Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | -45.0 °C | 100 % Show Supplier Material materials with Dehnung of 100 % | Min. |
23.0 °C | 600 % Show Supplier Material materials with Dehnung of 600 % | Min. | |
Kerbschlagenergie | 23.0 °C | 280 J Show Supplier Material materials with Kerbschlagenergie of 280 J | Min. |
Streckgrenze | 23.0 °C | 18 MPa Show Supplier Material materials with Streckgrenze of 18 MPa | Min., at 23°С |
Zugfestigkeit | 23.0 °C | 24 MPa Show Supplier Material materials with Zugfestigkeit of 24 MPa | Min., at 23°С |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | UKM is designed to protect the external anti-corrosion protective coating of the pipeline with a diameter of 225 to 1420 mm inclusively during laying, installation and during the entire period of pipeline operation. UKM covering material provides protection against external mechanical stress on pipeline surface underground, banked up with the conditional maximum allowable size of the soil fraction up to 150 mm. | |
Fillers | Glass Fiber |