Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 230 [-] Show Supplier Material materials with Härte, Brinell of 230 [-] | soft annealed |
Härte, Rockwell C | 50 - 58 [-] Show Supplier Material materials with Härte, Rockwell C of 50 - 58 [-] | |
Zugfestigkeit | 1665 - 2180 MPa Show Supplier Material materials with Zugfestigkeit of 1665 - 2180 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 1 % Show Supplier Material materials with Chrom of 1 % |
Eisen | Balance |
Kohlenstoff | 0.59 % Show Supplier Material materials with Kohlenstoff of 0.59 % |
Mangan | 0.9 % Show Supplier Material materials with Mangan of 0.9 % |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |
Vanadium | 0.1 % Show Supplier Material materials with Vanadium of 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Special steel for hand chisels of all types, including flat, cross-cut and pointed chisels for the treatment of hard materials; also for screwdrivers and other hand tools | |
Heat Treatment | Soft annealing: 710-740°C (Cooling in furnace) - Stress-relief-annealing: 650-680°C, Hardening: 810-850°C and quenching in oil |