Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 100 MPa Show Supplier Material materials with Biegefestigkeit of 100 MPa | ISO 178 |
Dehnung | 23.0 °C | 0.8 % Show Supplier Material materials with Dehnung of 0.8 % | ISO 178 |
Elastizitätsmodul | 23.0 °C | 15 GPa Show Supplier Material materials with Elastizitätsmodul of 15 GPa | ISO 178 (Flexural Test) |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 2 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 2 kJ/m² | ISO 179-1 |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 6 kJ/m² | ISO 179-1 |
Zugfestigkeit | 23.0 °C | 45 MPa Show Supplier Material materials with Zugfestigkeit of 45 MPa | ISO 527 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Glasübergangstemperatur | 200 °C Show Supplier Material materials with Glasübergangstemperatur of 200 °C | ISO 6721-7 | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | ISO 11359-2, Mean value for 20-105°C |
Wärmeleitfähigkeit | 23.0 °C | 0.7 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.7 W/(m·K) | ISO 8894 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 50Hz | 23.0 °C | 5.5 [-] Show Supplier Material materials with Dielectric constant, 50Hz of 5.5 [-] | IEC 60250 |
Kriechstromfestigkeit | 23.0 °C | 300 V Show Supplier Material materials with Kriechstromfestigkeit of 300 V | IEC 60112 |
Loss tangent, 50Hz | 23.0 °C | 1.5 [-] Show Supplier Material materials with Loss tangent, 50Hz of 1.5 [-] | IEC 60250 |
Surface resistivity | 23.0 °C | 16 Ω/sq Show Supplier Material materials with Surface resistivity of 16 Ω/sq | IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | High precision parts for automotive-, electrical- and general engineering | |
Fillers | Mineral Powder |