Allgemein
Property | Value | Testing Standard |
---|---|---|
Dichte | 1.07 g/cm³ Show Supplier Material materials with Dichte of 1.07 g/cm³ | ISO 1183-1 |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Biegefestigkeit | 70 MPa Show Supplier Material materials with Biegefestigkeit of 70 MPa | ISO 178 | 2 mm/min | |
Biegemodul | 2 GPa Show Supplier Material materials with Biegemodul of 2 GPa | ISO 527-1/2 | 2 mm/min | |
Dehnung | 30 % Show Supplier Material materials with Dehnung of 30 % | ISO 527-1/2 | 50 mm/min | |
Elastizitätsmodul | 2 GPa Show Supplier Material materials with Elastizitätsmodul of 2 GPa | ISO 527-1/2 | 1 mm/min | |
Elongation at yield | 3.7 % Show Supplier Material materials with Elongation at yield of 3.7 % | ISO 527-1/2 | 50 mm/min | |
Flexural strain | 15 % Show Supplier Material materials with Flexural strain of 15 % | ISO 527-1/2 | 50 mm/min | |
Hardness, Ball Indentation | 85 MPa Show Supplier Material materials with Hardness, Ball Indentation of 85 MPa | ISO 2039-1 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 30 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 30 kJ/m² | ISO 179-1eA | |
23 °C | 40 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 40 kJ/m² | ISO 179-1eA | ||
Schlagzähigkeit, Izod gekerbt | -30 °C | 34 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 34 kJ/m² | ISO 180-1A | |
23 °C | 42 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 42 kJ/m² | ISO 180-1A | ||
Streckgrenze | 45 MPa Show Supplier Material materials with Streckgrenze of 45 MPa | ISO 527-1/2 | 50 mm/min | |
Zugfestigkeit | 37 MPa Show Supplier Material materials with Zugfestigkeit of 37 MPa | ISO 527-1/2 | 50 mm/min |
Thermisch
Property | Value | Testing Standard | Pressure | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 700 °C Show Supplier Material materials with Glow Wire Flammability Index of 700 °C | IEC 60695-2-12 | 2.0 mm | ||||
Koeffizient der thermischen Ausdehnung | 9e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9e-05 1/K | ISO 11359-1/2 | 23 to 55°C | ||||
9e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9e-05 1/K | ISO 11359-1/2 | 23 to 55°C, Transverse | |||||
Vicat-Erweichungstemperatur | 106 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 106 °C | ISO 306 | 50 N | 50°C/h | ||||
Wärmeformbeständigkeitstemperatur | 99 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 99 °C | ISO 75-1/2 | 1.8 MPa | ||||
108 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 108 °C | ISO 75-1/2 | 0.45 MPa | |||||
Entflammbarkeit | At thickness 1.6 mm UL 94: HB. Burning rate US-FMVSS (2.0 mm): 34 mm/min | max. | according to ISO 3795 |
Elektrisch
Property | Value | Frequency | Testing Standard |
---|---|---|---|
Dielektrizitätskonstante | 3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3 [-] | 100Hz | IEC 60250 |
3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3 [-] | 1MHz | IEC 60250 | |
Surface resistivity | 2e+17 Ω/sq Show Supplier Material materials with Surface resistivity of 2e+17 Ω/sq | ||
Verlustfaktor | 0.0038 [-] Show Supplier Material materials with Verlustfaktor of 0.0038 [-] | 100Hz | IEC 60250 |
0.0086 [-] Show Supplier Material materials with Verlustfaktor of 0.0086 [-] | 1MHz | IEC 60250 | |
Volume resistivity | 6e+16 Ω·cm Show Supplier Material materials with Volume resistivity of 6e+16 Ω·cm | IEC 60093 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 14 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 14 cm³/10min | ISO 1133 | 260°C/5Kg |
Schrumpfung | 0.6 - 0.8 % Show Supplier Material materials with Schrumpfung of 0.6 - 0.8 % | ISO 2577 | 150x105x3 |
0.6 - 0.8 % Show Supplier Material materials with Schrumpfung of 0.6 - 0.8 % | ISO 2577 | 150x105x3, Transverse |
Technological properties
Property | ||
---|---|---|
Certifications | UL Certificate | |
Handling recommendations | Please see the Material Safety Data Sheet for relevant health & safety information. | |
Other | Control measurements in other places may issue different results due to influences of machinery, equipment, test method or storage conditions. | |
Processing methods | Injection molding-melt temperature: 240 ºC according to ISO 294 Injection molding-mold temperature: 70 ºC according to ISO 294 Injection molding-injection velocity: 240 mm/s according to ISO 294 |