Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.31 g/cm³ Show Supplier Material materials with Dichte of 1.31 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 80 MPa Show Supplier Material materials with Biegefestigkeit of 80 MPa | ISO 178 (2mm/min) |
Biegemodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Biegemodul of 2.5 GPa | ISO 178 (2mm/min) |
Dehnung | 23.0 °C | 200 % Show Supplier Material materials with Dehnung of 200 % | ISO 527-2 (5mm/min) |
Elastizitätsmodul | 23.0 °C | 2.9 GPa Show Supplier Material materials with Elastizitätsmodul of 2.9 GPa | ISO 527-2 (1mm/min) |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 220 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 220 kJ/m² | ISO 179/1eU |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 10 kJ/m² | ISO 180/1A |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 150 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 150 kJ/m² | ISO 180/1U |
Zugfestigkeit | 23.0 °C | 60 MPa Show Supplier Material materials with Zugfestigkeit of 60 MPa | ISO 527-2 (5mm/min) |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 160 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 160 °C | ISO 75-2/B | |
Heat deflection temperature, 1.80 MPa | 60 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 60 °C | ISO 75-2/A | |
Schmelzpunkt | 225 °C Show Supplier Material materials with Schmelzpunkt of 225 °C | ISO 3146 | |
Entflammbarkeit | UL94 (0.8mm) HB |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Kriechstromfestigkeit | 23.0 °C | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | EN 60112 |
Surface resistivity | 23.0 °C | 1.00E+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq | ASTM D257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 28 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 28 g/10min | ISO1133-1/2 (250°C/5 kg) | |
Schrumpfung | 23.0 °C | 1.8 % Show Supplier Material materials with Schrumpfung of 1.8 % | ISO 294-4 (3mm) |
Schrumpfung, diagonal | 23.0 °C | 2 % Show Supplier Material materials with Schrumpfung, diagonal of 2 % | ISO 294-4 (3mm) |
Technological properties
Property | ||
---|---|---|
Application areas | EPIMIX PBT is used in all sectors of industry, has and excellent surface finish, low warpage and all around excellent mechanical properties. | |
Other | Laboratory conditions are 23 ±2°C and 45-55 % RH. |