Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.75 g/cm³ Show Supplier Material materials with Dichte of 1.75 g/cm³ | ISO 1183 |
Water content | 23.0 °C | 0.2 % Show Supplier Material materials with Water content of 0.2 % | ISO 15512 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 250 MPa Show Supplier Material materials with Biegefestigkeit of 250 MPa | ISO 178 (2mm/min) |
Biegemodul | 23.0 °C | 12 GPa Show Supplier Material materials with Biegemodul of 12 GPa | ISO 178 (2mm/min) |
Dehnung | 23.0 °C | 1.5 % Show Supplier Material materials with Dehnung of 1.5 % | ISO 527-2 (5mm/min) |
Elastizitätsmodul | 23.0 °C | 12.5 GPa Show Supplier Material materials with Elastizitätsmodul of 12.5 GPa | ISO 527-2 (1mm/min) |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 65 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 65 kJ/m² | ISO 179/1eU |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 12 kJ/m² | ISO 180/1A |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 60 kJ/m² | ISO 180/1U |
Zugfestigkeit | 23.0 °C | 175 MPa Show Supplier Material materials with Zugfestigkeit of 175 MPa | ISO 527-2 (5mm/min) |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Aschegehalt | 23.0 °C | 40 % Show Supplier Material materials with Aschegehalt of 40 % | ISO 3451-4 | ||
Heat deflection temperature, 0.45 MPa | 215 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 215 °C | ISO 75-2/B | |||
Heat deflection temperature, 1.80 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 205 °C | ISO 75-2/A | |||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | ISO 3146 | |||
Ball Pressure Test | <2, for 125+/-2°C, EN 60695-10-2 | ||||
Entflammbarkeit | UL94 (0.8mm) V0, EN 60695-11-10 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Kriechstromfestigkeit | 23.0 °C | 250 V Show Supplier Material materials with Kriechstromfestigkeit of 250 V | EN 60112 |
Surface resistivity | 23.0 °C | 1.00E+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+14 Ω/sq | ASTM D257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Halogenated, compliance with RoHS derivatives, with rating UL94 V0 and glow-wire at 960°C, which is used in many sectors of industy and has excellent mechanical properties. | |
Certifications | RoHS | |
Fillers | 40% Glass Fiber | |
Other | Laboratory conditions are 23 ±2°C and 45-55 % RH. |