Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 3.45 g/cm³ Show Supplier Material materials with Dichte of 3.45 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 580 MPa Show Supplier Material materials with Biegefestigkeit of 580 MPa |
Elastizitätsmodul | 23.0 °C | 290 GPa Show Supplier Material materials with Elastizitätsmodul of 290 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 6.3 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 6.3 MPa·√m |