Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Supplier Material materials with Aluminium of 0.05 % |
Arsen | 0.02 - 0.15 % Show Supplier Material materials with Arsen of 0.02 - 0.15 % |
Blei | 1.7 - 2.8 % Show Supplier Material materials with Blei of 1.7 - 2.8 % |
Eisen | 0.1 % Show Supplier Material materials with Eisen of 0.1 % |
Kupfer | 61 - 63 % Show Supplier Material materials with Kupfer of 61 - 63 % |
Nickel | 0.3 % Show Supplier Material materials with Nickel of 0.3 % |
Zink | Balance, REM |