Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
EN CuZn38Pb2 Leaded Brass
Diese Materialdaten wurden von Fitco zur Verfügung gestellt
All categories
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Supplier Material materials with Aluminium of 0.05 % |
Blei | 1.6 - 2.5 % Show Supplier Material materials with Blei of 1.6 - 2.5 % |
Eisen | 0.2 % Show Supplier Material materials with Eisen of 0.2 % |
Kupfer | 60 - 61 % Show Supplier Material materials with Kupfer of 60 - 61 % |
Nickel | 0.3 % Show Supplier Material materials with Nickel of 0.3 % |
Zink | Balance, REM |
Zinn | 0.2 % Show Supplier Material materials with Zinn of 0.2 % |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.