Chemical properties
Property | Value |
---|---|
Aluminium | 0.3 - 1.3 % Show Supplier Material materials with Aluminium of 0.3 - 1.3 % |
Blei | 1 % Show Supplier Material materials with Blei of 1 % |
Eisen | 1 % Show Supplier Material materials with Eisen of 1 % |
Kupfer | 59 - 61.5 % Show Supplier Material materials with Kupfer of 59 - 61.5 % |
Mangan | 0.6 - 1.8 % Show Supplier Material materials with Mangan of 0.6 - 1.8 % |
Nickel | 0.6 % Show Supplier Material materials with Nickel of 0.6 % |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % |
Zink | Balance, REM |
Zinn | 0.3 % Show Supplier Material materials with Zinn of 0.3 % |