Chemical properties
Property | Value |
---|---|
Aluminium | 5 - 6 % Show Supplier Material materials with Aluminium of 5 - 6 % |
Blei | 0.2 - 0.8 % Show Supplier Material materials with Blei of 0.2 - 0.8 % |
Eisen | 2 - 3.5 % Show Supplier Material materials with Eisen of 2 - 3.5 % |
Kupfer | 63 - 65 % Show Supplier Material materials with Kupfer of 63 - 65 % |
Mangan | 3.5 - 5 % Show Supplier Material materials with Mangan of 3.5 - 5 % |
Nickel | 0.5 % Show Supplier Material materials with Nickel of 0.5 % |
Silizium | 0.2 % Show Supplier Material materials with Silizium of 0.2 % |
Zink | Balance, REM |
Zinn | 0.2 % Show Supplier Material materials with Zinn of 0.2 % |