Chemical properties
Property | Value |
---|---|
Aluminium | 4 - 5 % Show Supplier Material materials with Aluminium of 4 - 5 % |
Blei | 0.2 - 0.8 % Show Supplier Material materials with Blei of 0.2 - 0.8 % |
Eisen | 0.5 - 3 % Show Supplier Material materials with Eisen of 0.5 - 3 % |
Kupfer | 65 - 68 % Show Supplier Material materials with Kupfer of 65 - 68 % |
Mangan | 0.5 - 3 % Show Supplier Material materials with Mangan of 0.5 - 3 % |
Nickel | 1 % Show Supplier Material materials with Nickel of 1 % |
Zink | Balance, REM |