Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 3.21 g/cm³ Show Supplier Material materials with Dichte of 3.21 g/cm³ |
Partikelgrößenbereich | 100 µm Show Supplier Material materials with Partikelgrößenbereich of 100 µm | |
Schüttdichte | 23.0 °C | 0.86 g/cm³ Show Supplier Material materials with Schüttdichte of 0.86 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 23.0 °C | 24 GPa Show Supplier Material materials with Elastizitätsmodul of 24 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 4.5 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4.5 MPa·√m |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Halldurchfluss | 23.0 °C | 22.5 s/50g Show Supplier Material materials with Halldurchfluss of 22.5 s/50g |
Technological properties
Property | ||
---|---|---|
Application areas | Silicon Carbide Ready-To-Press granules for solid-state (SSiC) sintered technical ceramics. | |
Chemical composition | SiC type: SINTEX 13C; Al2O3: 5,5%; Y2O3: 3,5%; Moisture content: 1%; Binder content (total organic): 6% |