Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 11.8 - 12.4 g/cm³ Show Supplier Material materials with Dichte of 11.8 - 12.4 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Vickers, 10 | 23.0 °C | 150 - 200 [-] Show Supplier Material materials with Härte, Vickers, 10 of 150 - 200 [-] |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 2.60E+7 - 3.50E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 2.60E+7 - 3.50E+7 S/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 2E-3 % Show Supplier Material materials with Aluminium of 2E-3 % | Max. | |
Arsen | 2E-3 % Show Supplier Material materials with Arsen of 2E-3 % | Max. | |
Chrom | 2E-3 % Show Supplier Material materials with Chrom of 2E-3 % | Max. | |
Eisen | 3E-3 % Show Supplier Material materials with Eisen of 3E-3 % | Max. | |
Kalium | 1E-3 % Show Supplier Material materials with Kalium of 1E-3 % | Max. | |
Kalzium | 2E-3 % Show Supplier Material materials with Kalzium of 2E-3 % | Max. | |
Kobalt | 3E-3 % Show Supplier Material materials with Kobalt of 3E-3 % | Max. | |
Kohlenstoff | 5E-3 % Show Supplier Material materials with Kohlenstoff of 5E-3 % | Max. | |
Kupfer | 47 - 53 % Show Supplier Material materials with Kupfer of 47 - 53 % | ||
Magnesium | 2E-3 % Show Supplier Material materials with Magnesium of 2E-3 % | Max. | |
Molybdän | 5E-3 % Show Supplier Material materials with Molybdän of 5E-3 % | Max. | |
Natrium | 2E-3 % Show Supplier Material materials with Natrium of 2E-3 % | Max. | |
Nickel | 0.5 % Show Supplier Material materials with Nickel of 0.5 % | Max. | |
Schwefel | 2E-3 % Show Supplier Material materials with Schwefel of 2E-3 % | Max. | |
Silizium | 3E-3 % Show Supplier Material materials with Silizium of 3E-3 % | Max. | |
Wolfram | balance |
Technological properties
Property | ||
---|---|---|
Application areas | EDM electrode material for spark erosion; Resistance and contact welding electrode material; Contact material for electrical engineering; Material to balance rotating systems |