Abmessung
Property | Value |
---|---|
Dimensions | <p>Standard process capabilities:</p> <p>Width: 10-1400mm</p> <p>Thickness 0.050-3.18mm</p> |
Mechanisch
Property | Value | Comment |
---|---|---|
Streckgrenze | 160 MPa Show Supplier Material materials with Streckgrenze of 160 MPa | RP02 |
Zugfestigkeit | 180 - 220 MPa Show Supplier Material materials with Zugfestigkeit of 180 - 220 MPa |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 635 - 655 °C Show Supplier Material materials with Schmelzpunkt of 635 - 655 °C |
Elektrisch
Property | Value | Comment |
---|---|---|
Korrosionspotenzial | -800 mV Show Supplier Material materials with Korrosionspotenzial of -800 mV | |
spezifischer Widerstand | 3.4e-08 - 4.3e-08 Ω·m Show Supplier Material materials with spezifischer Widerstand of 3.4e-08 - 4.3e-08 Ω·m | Changes depending on temper |
Chemical properties
Property | Value |
---|---|
Aluminium | Balance |
Eisen | 0 - 0.4 % Show Supplier Material materials with Eisen of 0 - 0.4 % |
Kupfer | 0 - 0.05 % Show Supplier Material materials with Kupfer of 0 - 0.05 % |
Magnesium | 0 - 0.05 % Show Supplier Material materials with Magnesium of 0 - 0.05 % |
Mangan | 1.4 - 1.8 % Show Supplier Material materials with Mangan of 1.4 - 1.8 % |
Silizium | 0.65 - 1 % Show Supplier Material materials with Silizium of 0.65 - 1 % |
Zink | 1.3 - 1.7 % Show Supplier Material materials with Zink of 1.3 - 1.7 % |
Zirkonium | 0.05 - 0.2 % Show Supplier Material materials with Zirkonium of 0.05 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, Heat Exchangers | |
Processing history | Temper: H14SR |